UNS S21640 austenitic chromium-manganese-nickel stainless steel
Chemical composition, % UNSdesignation S21800 Type – Carbon 0.08 Manganese 3.50–6.50 Phosphorus 0.060 Sulfur 0.030 Silicon 1.00 Chromium 17.5–19.5 Nickel
Continue readingGuide of steels, alloys, precious metals and other materials
Chemical composition, % UNSdesignation S21800 Type – Carbon 0.08 Manganese 3.50–6.50 Phosphorus 0.060 Sulfur 0.030 Silicon 1.00 Chromium 17.5–19.5 Nickel
Continue readingEquivalents USAAISI 301 USA(SAE) 30301 USAUNS S30100 Germany(№/DIN) 1.4310/X12CrNi177 ISO Type-14 India (IS) 10Cr17Ni7 JIS SUS301 GBRBS970 310S21 FRANFA35 Z12CN17-07
Continue readingChemical composition, % UNSdesignation S21800 Type Nitronic 60 Carbon 0.10 Manganese 7.00-9.00 Phosphorus 0.060 Sulfur 0.030 Silicon 3.5–4.5 Chromium 16.0–18.0
Continue readingDescription AISI 410 (UNS Number S41000) the most widely used martensitic (plain chromium stainless class with exceptional strength) stainless steel,
Continue readingEquivalents CountryStandard Gradeor Name EN10016-2 (1995) C4D(1.0300) EN10016-4 (1995) C3D2(1.1110) Chemical composition, % Grade (AISI/SAE) 1005 UNS No. G10050 Carbon
Continue readingEquivalents BS/UK 420S29,420S37 DIN/Germany 1.4021 NF/France Z20 C13 SS/Sweden 2303 GB/PR China 2Cr13 India 20Cr13 KS/Korea STS 420J1 GOST/Russia 20X13
Continue readingEquivalents CountryStandard Gradeor Name EN10016-2 (1995) C9D(1.0304) EN10016-4 (1995) C8D2(1.1113) RussiaGOST 0808kp08ps Chemical composition, % Grade (AISI/SAE) 1008 UNS No.
Continue readingEquivalents CountryStandard Gradeor Name EuropeEN 10016-2(1995) C18D(1.0416) JapanJIS G4051(1979) S17C Chemical composition, % Grade (AISI/SAE) 1008 UNS No. G10080 Carbon
Continue readingHot working and heat treatment Forging: 1200°C Max. (Commence), 850°C Min. (Finish) Annealing: Heat to 800°C (Furnace cooled at a
Continue readingHot working and heat treatment Forging: 1200°C Max. (Commence), 850°C Min. (Finish) Annealing: Heat to 845°C furnace cool at a